Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 140 GM Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values.. |
|||
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet.. |
|||
Bulk Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 FS Dense Refractory Castable Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | |
MarkeTech Repton 922 Yttria Y2O3 REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | |
Sharadaa Ceramics MH 30 Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF40 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | >= 2.00 g/cc | >= 0.0723 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST C SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | |
Sharadaa Ceramics REFCAST Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | >= 2.00 g/cc | >= 0.0723 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | >= 2.00 g/cc | >= 0.0723 lb/in³ | Sample, cast, cured, dried at 110°C |
Sharadaa Ceramics REFCAST NORMAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | As supplied |
Zircar Zirconia ZR-CEM Zirconia Cement Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zi.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | |
Du-Co Ceramics S-570 Silica Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Bulk Density | >= 2.00 g/cc | >= 0.0723 lb/in³ | |
China-Yixing Longly Refractories ASM-125 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | |
Chosun Refractories ALB-65I Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.00 - 2.16 g/cc | 0.0723 - 0.0781 lb/in³ | |
ATI Wah Chang Hafnium Oxide, HfO2 A free flowing, coarse, tan powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |
|||
Bulk Density | 2.00 - 2.04 g/cc | 0.0723 - 0.0737 lb/in³ | |
Ceradyne Thermo-Sil® Isomolded™ Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
Bulk Density | 2.00 g/cc | 0.0723 lb/in³ | As supplied |
Zircar Zirconia ZR-CEM Zirconia Cement Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zi.. |