Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 FS Dense Refractory Castable Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f.. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar.. |
|||
Thermal Conductivity | 1.10 - 1.20 W/m-K @Temperature 100 °C |
7.63 - 8.33 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |