Thermal Conductivity 1.16 - 1.26 W/m-K

@Temperature 1000 °C
8.05 - 8.74 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 160 FS Dense Refractory Castable
Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f..