Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 2.10 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 130 Dense Refractory Castable
Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap..
Bulk Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 140 GM Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values..
Bulk Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable
Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet..
Bulk Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 160 FS Dense Refractory Castable
Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f..
Copyright © lookpolymers.com All Rights Reserved