Material Notes:
Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.80 - 1.90 g/cc
0.0650 - 0.0686 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 15.0 - 25.0 MPa

@Temperature 1000 °C
2180 - 3630 psi

@Temperature 1830 °F
Cold Crushing Strength
25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.490 - 0.590 W/m-K

@Temperature 600 °C
3.40 - 4.09 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.530 - 0.630 W/m-K

@Temperature 1000 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Shrinkage -0.200 - 0.000 %

@Temperature 1000 °C
-0.200 - 0.000 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 30 %
30 %
SiO2 53 %
53 %
Descriptive Properties Value Comments
ASTM Classification A
Material Consumption per 1 m3 1800 kg
Mixing Water 15-18 liters
per 100 kgs dry material