Polymer Property : Bulk Density = 0.0650 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.80 g/cc
0.0650 lb/in³
MarkeTech Repton 202 Aluminum Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
Bulk Density 1.80 - 1.90 g/cc
0.0650 - 0.0686 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 110 Dense Refractory Castable
Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a..
Bulk Density 1.80 - 1.90 g/cc
0.0650 - 0.0686 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 145 P Dense Refractory Castable
Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas..
Bulk Density 1.80 g/cc
0.0650 lb/in³
of Dry Beads
Mo-Sci Corporation GL-0176 Barium-Titanate Glass Spheres
Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0176 beads include: high temperature spacer material for gauge control, coating, filler for plas..
Bulk Density 1.80 g/cc
0.0650 lb/in³
of Dry Beads
Mo-Sci Corporation GL-0275-B Class VI Barium-Titanate Glass Spheres
Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0275-B beads including: high temperature spacer material for gauge control, coating, filler for ..
Bulk Density >= 1.80 g/cc
>= 0.0650 lb/in³
Sample, cast, cured, dried at 110°C
Sharadaa Ceramics REFCAST LT Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Bulk Density 1.80 g/cc
0.0650 lb/in³
Chosun Refractories AIN-1 Special brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 1.80 g/cc
0.0650 lb/in³
of Dry Beads
Mo-Sci Corporation GL-0175 Barium-Titanate Glass Spheres
Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0175 beads include:: high temperature spacer material for gauge control, coating, filler for pla..
Bulk Density 1.80 g/cc
0.0650 lb/in³
Effective Density measured in SAE 20 motor oil using Gardner cup
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere
Fine particle white spheres developed as filler for paints, coatings and films.Information provided by Potters Industries.