Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 15.0 - 25.0 MPa @Temperature 1000 °C |
2180 - 3630 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 110 Dense Refractory Castable Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a.. |