Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Pyrotek RFM Light density refractory composite material The RFM material is a composite made of fiberglass fabric and a wollastonite slurry. It can be shaped to very complex and thin parts. It has a very good behavior against molten aluminum alloys.App.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | Recommended for use in continuous casting applications |
Pyrotek Pyrocast 220HT Refractory Castable Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Gouda Vuurvast GOLITE 110 Refractory Insulating Castable Description: Golite 110 is composed of a light weight refractory aggregate plus several additives to improve the mechanical and refractory properties.Remarks: These values apply to cast products. Al.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Skamol Group SKAMOLEX V-1100 (700) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Skamol Group V-1100 375 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Skamol Group V-1100 410 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Skamol Group V-1100 600 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Skamol Group VERMICAST 14-100 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® HSA (OF) Ceramic Fiber Paper HSA paper is made from high surface area (HSA) fibers that contain a low percentage of unfiberized material. Use of this fiber results in a paper with lighter weight and extremely low thermal condu.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor du.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | Recommended Operating Temperature |
Unifrax Insulfrax® 1100C Modules Insulfrax® 1100C Modules are a family of high-temperature module products based on Unifrax's Anchor-Loc® attachment systems. Modules used in the Anchor-Loc® systems are constructed with Insulfra.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® 972-H Ceramic Fiber Paper This product is completely free of organics and used when higher fired strength is required or in processes and applications where even small amounts of organic burnout is unacceptable. 972-H is he.. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Goodfellow T1-Thermocouple Alloy The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also .. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Chosun Refractories 1000BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | limited |
Chosun Refractories GUN-110L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | limited |
Chosun Refractories INCT-110N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | limited |
Chosun Refractories INCT-110S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® 970 Ceramic Fiber Paper 970 paper is made from high-purity Fiberfrax washed fiber. During the manufacture of this product, a large portion of the unfiberized particles in the bulk fiber are removed prior to paper lay-up. .. |
|||
Maximum Service Temperature, Air | 1100 °C | 2010 °F | |
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |