Compressive Strength 15.0 - 25.0 MPa

@Temperature 1000 °C
2180 - 3630 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 110 Dense Refractory Castable
Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a..