Thermal Properties Metric English Comments
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 110 C Dense Refractory Castable
Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 110 Dense Refractory Castable
Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a..
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 1000 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 145 P Dense Refractory Castable
Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas..
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 1000 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast...
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 1260 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 2300 °F
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari..
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 100 Dense Refractory Castable
Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification..
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 100 C Dense Refractory Castable
Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values ..
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 1000 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 35-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.