Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer GEHR Plastics Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional stability, and creep strength. The LOI belongs to the highest of polymers. By the reinforcement with glass polymers strength is achieved, which is comparable with light metal. PPS closes the gap between the technical synthetics and PEEK with its strength and economy.Propertiesvery high strength and rigidityhigh hardnesshigh thermostabilityhigh dimensional stabilityvery high chemical resistancevery good insulating propertieshigh weather resistancehigh resistance to hydrolysisApplications include components in machine-making, pump parts, fan parts, impellers, parts in the fuel and automotive sector.
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
Ball Indentation Hardness 322 MPa
46700 psi
ISO 2039
Tensile Strength at Break 185 MPa
26800 psi
ISO 527
Elongation at Break 1.9 %
1.9 %
ISO 527
Modulus of Elasticity 14.0 GPa
2030 ksi
ISO 527
Flexural Strength 285 MPa
41300 psi
3.5%; ISO 178
Charpy Impact Unnotched 5.30 J/cm²
25.2 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179
Coefficient of Friction 0.40
0.40
DIN 53375
Thermal Properties Metric English Comments
CTE, linear 48.0 µm/m-°C

@Temperature 20.0 °C
26.7 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 240 °C
464 °F
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ISO 75
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
VDE 0303
Surface Resistivity per Square >= 1.00e+15 ohm
>= 1.00e+15 ohm
VDE 0303
Dielectric Constant 4.1

@Frequency 1.00e+6 Hz
4.1

@Frequency 1.00e+6 Hz
DIN 53483
Dielectric Strength 28.0 kV/mm
711 kV/in
VDE 0303
Dielectric Loss Index 0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
DIN 53483
Comparative Tracking Index 125 V
125 V
CTI; IEC 60112
Descriptive Properties Value Comments
Acid Resistance yes
Aromatic Resistance limited
Bondability yes
CKW Resistance yes
Color Black
Hydrocarbonate Resistance yes
Hydroxide Resistance limited
Ketone Resistance limited
Physiological indifference according yes
Resistance Against Hot Water limited
UV Stabilization yes