Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet) Natural and Black |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | ASTM D257 |
PolyOne Edgetek® PS-20GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PEI Polyetherimide Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Wanshijie PC Film PC is a kind of shapeless, odorless, non-toxic, high transparency, colorless or light yellow thermoplastic engineering plastic with excellent physical and mechanical properties, especially excellent.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | ASTM D257 |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® 475 Polyester Film, 200 Gauge Melinex® 475 is a high yield, translucent polyester film with superb handling properties. Both surfaces are pretreated to promote adhesion to most industrial coatings.General Product Info: This fil.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Non-adhesive side; ASTM D257 |
3M 4104 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Adhesive side; ASTM D257 |
3M 4104 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Adhesive side; ASTM D257 |
3M 4108 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |