Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Elongation at Break >= 7.0 %
>= 7.0 %
ASTM D638
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
ASTM D648