Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

G-3 Fiberglass Phenolic Laminate Sheet

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic/Glass Fiber SMC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF G-3 Fiberglass Phenolic Laminate Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of fabrication, and excellent electrical properties make phenolic laminates useful as support components in a wide range of mechanical and electrical applications. Phenolic laminates are strong, stiff, and have high impact and compressive strengths. They do not soften upon re-heating, so they are easy to saw, drill, tap, and machine with ordinary tools. Glass-based grades have the highest dimensional stability and mechanical strength, as well as low moisture absorption. However, they are not as easily machined as paper or cotton fabric laminates. Information provide by Boedeker Plastics.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 2.65 %
2.65 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 110
110
ASTM D785
Tensile Strength at Break 234 MPa
34000 psi
Crosswise; ASTM D638
290 MPa
42000 psi
Lengthwise; ASTM D638
Flexural Strength 234 MPa
34000 psi
Crosswise; ASTM D790
279 MPa
40500 psi
Lengthwise; ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
Crosswise; ASTM D790
12.4 GPa
1800 ksi
Lengthwise; ASTM D790
Compressive Strength 379 MPa
55000 psi
ASTM D695
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
Crosswise; ASTM D256
6.41 J/cm
12.0 ft-lb/in
Lengthwise; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 14.9 µm/m-°C

@Temperature 20.0 °C
8.30 µin/in-°F

@Temperature 68.0 °F
Lengthwise; ASTM D696
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
Thermal Conductivity 0.288 W/m-K
2.00 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 170 °C
338 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 7.3

@Frequency 1e+6 Hz
7.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.1 kV/mm
460 kV/in
Short Time; 1/8 inch; ASTM D149
Dissipation Factor 0.023

@Frequency 1e+6 Hz
0.023

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Users viewing this material also viewed the following: