Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding 40% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 66, 35% Glass Filled
(discontinued **) Heat Stabilized, Hydrolysis Resistant in Automotive CoolantInformation provided by Ravago. |
|||
Flexural Modulus | 9.65 - 27.6 GPa | 1400 - 4000 ksi | Average value: 19.4 GPa Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF33 TL15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES HiFill® PBT WM35 X Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU (Asia Pacific) LNP* Thermocomp* GX05482 is a compound based on Polysulfone resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Ecomass® 1850ZG90 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Flexural Modulus | 9.65 GPa @Temperature 22.8 °C |
1400 ksi @Temperature 73.0 °F |
Tangent; ASTM D790 |
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK) TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Ensinger Tecapeek® XP-181 Compression Molded PPEK Compound, EWS Filled and Carbon Fiber Reinforced Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 9.65 - 11.0 GPa | 1400 - 1600 ksi | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |