Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
PolyOne LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ISO 178 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Flexural Modulus | 9.67 GPa | 1400 ksi | ASTM Data |
BASF Capron® SEG7 35% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron SEG7 is an unfilled injection molding type 6 nylon graft copolymer. It has superior impact resistance and flow especially for thinner walled parts and long flow lengths. Copolymerization res.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
PolyOne Edgetek® PS-30GF/000 FR V0 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 6/6, 35% Fiberglass (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | Crosswise; ASTM D790 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 5105 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU (Asia Pacific) LNP* Thermocomp* GX05482 is a compound based on Polysulfone resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 LNP* THERMOCOMP* QF0069 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific) LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Clariant PA612G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Clariant PA621G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | Secant at 0.5 Deflection; ASTM D790 |
Applied Composites 179 Polyester SMC Industry Application: TransportationProduct Application: Auto InteriorsInformation provided by Applied Composites Corporation. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | Tangent; ASTM D790 |
Applied Composites 8012 Polyester SMC Industry Application: SpecialtyProduct Application: Food EquipmentDistinct Features: NSF ApprovedInformation provided by Applied Composites Corporation. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan.. |
|||
Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |