Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 290 MPa | 42100 psi | ISO 527-2 |
PolyOne OnForce™ LFT NN-30LCF/002 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Strength at Break | 290 MPa | 42000 psi | Lengthwise; ASTM D638 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Tensile Strength at Break | 290 - 338 MPa | 42000 - 49000 psi | Wire, Temper- Hard |
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and .. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50 Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-6H nat PA*-GF60 Product description: Grivory GVL-6H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H na.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70 Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70 Product description: Grivory GVX-7H natural is a 70% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60 Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60 Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Tensile Strength at Break | 290 MPa | 42100 psi | 5 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Strength at Break | 290 MPa @Temperature 760 °C |
42100 psi @Temperature 1400 °F |
Solution Annealed Tubing |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |