Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum PPS Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | 0.288 - 0.400 W/m-K | 2.00 - 2.78 BTU-in/hr-ft²-°F | Average value: 0.336 W/m-K Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Thermal Conductivity | 0.289 W/m-K | 2.00 BTU-in/hr-ft²-°F | Laser Flash Method |
UBE UPILEX 75S (75 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |
|||
Thermal Conductivity | 0.289 W/m-K | 2.00 BTU-in/hr-ft²-°F | Laser Flash Method |
UBE UPILEX 25S (25 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | |
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base Single component system with a paint consistency. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | 0.288 - 0.380 W/m-K | 2.00 - 2.64 BTU-in/hr-ft²-°F | Average value: 0.321 W/m-K Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | ASTM C177 |
G-5 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and .. |
|||
Thermal Conductivity | 0.288 - 22.0 W/m-K | 2.00 - 153 BTU-in/hr-ft²-°F | Average value: 5.71 W/m-K Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Thermal Conductivity | 0.288 - 1.21 W/m-K | 2.00 - 8.40 BTU-in/hr-ft²-°F | Average value: 0.442 W/m-K Grade Count:6 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Thermal Conductivity | 0.288 W/m-K | 2.00 BTU-in/hr-ft²-°F | |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |