Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for injection molding including thin wall applications. The use of an advanced clarifier with low yellowness index and haze – makes it an excellent choice for ‘see-through’ housewares and rigid packaging. Use of this clarifier allows processers to run at lower temperatures - resulting in the potential for cycle time reductions and energy savings Formolene® 3355E meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact. Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 55 g/10 min

@Temperature 230 °C
55 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4200 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 15 %
15 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature 23.0 °C
1.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Gardner Impact 20.0 J
14.8 ft-lb
ASTM D5420
20.3 J
15.0 ft-lb
ASTM D2794
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 178 °C
352 °F
ASTM D648
Optical Properties Metric English Comments
Haze 10 %

@Thickness 1.00 mm
10 %

@Thickness 0.0394 in
Plaque; FPC method