Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 0710 C Brown Polypropylene Data provided by Multibase. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT2400-648UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 5002 X White 50% Filler Content Polypropylene Multi-Pro 5002 X White is an extrusion grade filled polypropylene that has good stiffness as well as excellent impact properties. It can be made in any color.Data provided by Multibase. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D5420 |
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 20.3 J @Thickness 3.17 mm, Temperature 23.0 °C |
15.0 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D3029 |
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global) Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig.. |
|||
Gardner Impact | 20.3 J | 15.0 ft-lb | ASTM D2794 |
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje.. |
|||
Gardner Impact | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
1/2" R Tup, 180 mil |
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4526 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high res.. |