Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 20.0 J | 14.8 ft-lb | ASTM D3029 |
LyondellBasell Astryn BB725GC Polypropylene Copolymer, Mineral Filled Key Features: medium melt flow, medium high modulus, UV-stabilized, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good processability, good weatherability,Applicati.. |
|||
Gardner Impact | 20.0 J | 14.8 ft-lb | ASTM D5420 |
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje.. |