Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ASTM D648 |
Network Polymers Nylon 0304NL Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ISO 75 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ASTM D648 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ISO 75 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ISO 75 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C @Thickness 3.20 mm |
352 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12 LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 E HS N Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Nucleating AgentFeatures: Heat Stabilized and NucleatedProcessing Method: ExtrusionTPCI# 9587102Information provided by TP Comp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 E U Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: ExtrusionTPCI# 9777102Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 E2 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 E40 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 HS L BK Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackTPCI# 7190102Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 HS L Colors Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: Colors AvailableTPCI# 10014102Information provided by TP Composite.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 HS YL030 Heat Stabilized Availability: North AmericaForms: PelletsFeatures: Fast Molding Cycle and Good AdhesionAppearance: YellowTPCI# 10054102Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L LE MB Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low ExtractablesAppearance: Colors AvailableTPCI# 7964102Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L N MB (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L N YL038MB Availability: North AmericaForms: PelletsAdditive: Lubricant, UV Stabilizer and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Good UV Resistance and NucleatedAppeara.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 NAT Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 1026102Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 X BN071 EL MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Fast Molding Cycle, Good Processability, Lubricated and NucleatedTPCI# 1033102Information provided by TP Co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 E M/SL4 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant and Silicone LubricantFeatures: Low Friction, Good Wear Resistance and LubricatedAppearance: BlackInformation provid.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C @Thickness 3.20 mm |
352 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6 L N BK MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Fast Molding Cycle, Good Processability, Nucleated and LubricatedTPCI# 7970102Information provided by TP Co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6 L N BK002 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and Lubricant(4500 ppm)Features: Fast Molding Cycle, Good Processability, Nucleated and LubricatedAppearance: BlackTPCI# 1327102In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 HS L Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 7190102Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C @Thickness 3.20 mm |
352 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOTUF VX99809 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ASTM D648 |
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ASTM Test |
BASF Ultramid® 8202 HS BK-102 PA6 (Dry) Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses .. |