Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 190 °C |
55 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
Multibase TPSiV® 4000-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NCMT NanoPAC™ HS402 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Reliance Industries Repol B550MN Polypropylene REPOL Polypropylene B550MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | ASTM D1238 |
ExxonMobil Santoprene® 912BA Thermoplastic Elastomer
(discontinued **) A hard, black, super high-flow thermoplastic olefin (TPO) in the thermoplastic elastomer (TPE) family. This grade of Vistaflex TPE is temperature-dependent and can be processed on conventional therm.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9055 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | 55 cm<sup>3</sup>/10 min; Melt Volume Rate |
Huntsman IROGRAN® A 85 P 4394 FCM Ether-Based TPU-For Food Contact Extrusion grade; High microbial resistance, high transparencyInformation provided by Huntsman |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | ASTM D1238 |
Flint Hills AP5155-HA Polypropylene Impact Copolymer Features: Excellent processability, nucleated and Antistat.Applications: Injection molding: thin wall parts, food containers, packaging and medicalInformation Provided by Flint Hills Resources |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R55C-00 Clarified Polypropylene Copolymer Grade R55C-00 is a high melt flow rate clarified and antistatic random polypropylene copolymer. It is designed for high speed injection molding of thin walled parts requiring very good mold filling .. |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 266 °C |
55 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 300 °C |
55 g/10 min @Load 22.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 300 °C |
55 g/10 min @Load 22.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1550GN15 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN15 is a reinforced, flame retardant (.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HJ320MO Polypropylene HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is .. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 - 60 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 - 60 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 55 g/10 min @Temperature 230 °C |
55 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje.. |
|||
Melt Flow | 55 g/10 min @Temperature 230 °C |
55 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3355O Random Copolymer Polypropylene Random Copolymer for Clear Storage Containers and Food and Beverage Containers Formolene® 3355O is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for i.. |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D 1238 |
Cossa Polimeri ESTAPROP HK 4000 CH-HT Polypropylene Copolymer Polypropylene copolymer, high fluidityInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® W 77 AV Polypropylene Homopolymer CAPILENE® W 77 AV is a very high melt flow rate polypropylene homopolymer for injection molding with antistatic and nucleating additives. It offers a good balance of stiffness and flow, high de-mol.. |
|||
Melt Flow | 55 - 65 g/10 min | 55 - 65 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1084 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |