Fainplast Compounds RKS 310/K1 Rigid PVC, Antishock Extrusion Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds RKS 310/K1 Rigid PVC, Antishock Extrusion Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mat effect antishock profiles
Physical Properties Metric English Comments
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ISO R 527
Tensile Strength, Yield 38.0 MPa
5510 psi
ISO R527
Elongation at Break 80 %
80 %
ISO R 527
Izod Impact, Unnotched 0.800 - 1.20 J/cm

@Temperature 23.0 °C
1.50 - 2.25 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 79.0 - 81.0 °C

@Load 5.00 kg
174 - 178 °F

@Load 11.0 lb
ISO R306