Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Bynel® 3030 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont™ Surlyn® 1652SBR Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652SBR is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to pro.. |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 412/L Rigid PVC, Extrusion Corrugated plastics |
|||
Vicat Softening Point | 79.0 °C | 174 °F | |
LyondellBasell Lupolen® 5621 D HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 059/1 Rigid PVC, Injection Molding Fittings high fluidity |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 55 Rigid PVC, Injection Molding Fittings for building trade - high fluidity |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RL 455/AB Rigid PVC, Antishock Extrusion Corrugated antishock electric pipes |
|||
Vicat Softening Point | 79.0 °C | 174 °F | B120; ISO 306 |
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer INNOPOL® CS 2-8000 is a polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8000 is highly suitable for pipe manufacturing where the required.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | B120; ISO 306 |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 670 Ethylene Vinyl Acetate DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film 9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating 9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | A50; ISO 306 |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Nucrel® AE High Performance Adhesive and Sealant Resin Nucrel® Nucrel® AE is a terpolymer of ethylene, methacrylic acid, and acrylate, available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designe.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 5kg load; ISO 306 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 1kg load; ASTM D1525 |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | |
Covestro Desmopan® 372 Thermoplastic Polyurethane Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525, ISO 306 |
DuPont™ Nucrel® 3990L Ethylene Acrylic Acid Nucrel® 3990L is a copolymer of ethylene and acrylic acid. It is available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment. 9.5 % By Weight Acrylic.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
Braskem PB 608 LDPE Injection Molding Polyethylene Description: PB608 is a grade produced under high pressure in an autoclave reactor. This grade is especially designed for injection molding of articles that must show excellent flexibility propertie.. |
|||
Vicat Softening Point | 79.0 °C @Load 1.02 kg |
174 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem TN2020 EVA General Film Copolymer TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1010 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, transparent films with high mechanical properties. Examples: stretch film, food packaging.ISO data provided by t.. |
|||
Vicat Softening Point | 78.9 °C | 174 °F | ASTM D1525 |
Teknor Apex Sinvicomp DFR 5806 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 50°C/hr; 50N |
Arkema Group Kynar® FLEX 2800 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 2901 Medium Impact Polystyrene
(discontinued **) LACQRENE® 2901 is a very easy flowing, medium impact polystyrene for injection molding. The very high flow of this grade allows for the production of thin wall section or long flow path molding on.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | temperature B; ISO 36 |
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |