Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont™ Surlyn® 1652SBR Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652SBR is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to pro.. |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 412/L Rigid PVC, Extrusion Corrugated plastics |
|||
Vicat Softening Point | 79.0 °C | 174 °F | |
LyondellBasell Lupolen® 5621 D HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 059/1 Rigid PVC, Injection Molding Fittings high fluidity |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 320 Rigid PVC, Extrusion Lead Free Indoor profiles |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 218/W Rigid PVC, Antishock Extrusion Lead Free Antishock profiles |
|||
Vicat Softening Point | 79.0 - 81.0 °C @Load 5.00 kg |
174 - 178 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RL 455/AB Rigid PVC, Antishock Extrusion Corrugated antishock electric pipes |
|||
Vicat Softening Point | 79.0 °C | 174 °F | B120; ISO 306 |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Vicat Softening Point | >= 79.0 °C | >= 174 °F | ASTM D 1525 |
Karina 806-18/364-BY-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 79.0 °C | >= 174 °F | ASTM D 1525 |
Karina 837-10/119-E-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
Spartech Royalite R61M Low Smoke Resin Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 670 Ethylene Vinyl Acetate DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film 9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating 9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ISO 306 |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | A50; ISO 306 |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont Nucrel® AE High Performance Adhesive and Sealant Resin Nucrel® Nucrel® AE is a terpolymer of ethylene, methacrylic acid, and acrylate, available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designe.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 5kg load; ISO 306 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 1kg load; ASTM D1525 |
Eastman Provista UVO Copolymer Provista UVO is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | |
Dow ATTANE™ 4403 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4403 copolymer is an ultra low density polyethylene having high impact, tear strength and exceptional flexibility. It is designed for use in industrial/consumer blown film applications and .. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
Braskem PB 608 LDPE Injection Molding Polyethylene Description: PB608 is a grade produced under high pressure in an autoclave reactor. This grade is especially designed for injection molding of articles that must show excellent flexibility propertie.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1010 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, transparent films with high mechanical properties. Examples: stretch film, food packaging.ISO data provided by t.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 50°C/hr; 50N |
Arkema Group Kynar® FLEX 2800 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
DuPont™ Surlyn® 1652SR Zinc Ionomer Resin for Cast Film and Extrusion Coating Surlyn® 1652SR is an ionomer resin available for use in cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resi.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 2901 Medium Impact Polystyrene
(discontinued **) LACQRENE® 2901 is a very easy flowing, medium impact polystyrene for injection molding. The very high flow of this grade allows for the production of thin wall section or long flow path molding on.. |
|||
Vicat Softening Point | 79.0 °C | 174 °F | temperature B; ISO 36 |
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Vicat Softening Point | 79.0 - 205 °C | 174 - 401 °F | Average value: 126 °C Grade Count:44 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |