Material Notes:
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult injection molding applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Key Features: Used in glass encapsulation applicationsUsed in sealing applications.Recommended for applications requiring superior part surface appearance.Designed to be injected at lower molding temperatures or at lower injection pressures.EU and China RoHS compliant.Applications:Automotive-Glass Encapsulation and Weather SealsUses:Automotive ApplicationsAutomotive Interior Trim Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
2 mm, 15 sec; ISO 868
Tensile Strength at Break 4.83 MPa
700 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 2.00 MPa
290 psi
Across Flow; ASTM D412
Elongation at Break 480 %
480 %
Across Flow; ASTM D412
Compression Set 29 %
29 %
73°F, 70 hr; ASTM D395
56 %
56 %
257°F, 70 hr; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 79
Color Black
Form Pellets