Material Notes:
Texaco Hydraulic Safety Fluid is a fire-resistant fluid designed for use in high pressure hydraulic systems where the requirements for fire resistance, pump wear protection and viscosity are satisfied by water-glycol fluids.Texaco Hydraulic Safety Fluid is a water solution of diethylene glycol containing antiwear agents and rust inhibitors.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:The following table can be used with acceptable accuracy to determine the amount of water required to adjust the fluid to acceptable limits. Only distilled or deionized water should be used as makeup. The use of hard tap water, well or spring water should be avoided since the dissolved minerals in these waters will react with the additive system in the fluid to cause fluid haziness and formation of soap-like insoluble material.Fluid with a viscosity below 36.2 cSt at 40°C, or Brix readings below 42, contain excess water and only new Texaco Hydraulic Safety Fluid should be used as makeup. This chart is only valid when the system contains all Texaco Hydraulic Safety Fluid.Water adjustment, gallons per 100 gallons of fluidCPS Number: 220766; MSDS Number: 10587
Physical Properties Metric English Comments
API Gravity -1.70 °
-1.70 °
Viscosity Measurement 201
201
Viscosity Index
Saybolt Viscosity at 100°F 227 SUS
227 SUS
Saybolt Viscosity at 210°F 55.7 SUS
55.7 SUS
Kinematic Viscosity at 40°C (104°F) 41 cSt
41 cSt
Kinematic Viscosity at 100°C (212°F) 8.8 cSt
8.8 cSt
Thermal Properties Metric English Comments
Pour Point -74.0 °C
-101 °F
Processing Properties Metric English Comments
Moisture Content 40 %
40 %
vol%
Descriptive Properties Value Comments
Brix Number 42-44.5
38.5 - 41.4% H2O
45
37.7% H2O, 2 gal. adjustment, See Notes 1, 2
46
36.3% H2O, 4 gal. adjustment, See Notes 1, 2
47
34.7% H2O, 7 gal. adjustment, See Notes 1, 2
48
33.3% H2O, 10 gal. adjustment, See Notes 1, 2
49
31.7% H2O, 12 gal. adjustment, See Notes 1, 2
50
30.3% H2O, 14 gal. adjustment, See Notes 1, 2