Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | ISO 37 |
Multibase TPSiV® 4200-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | ASTM D412 |
Objet FullCure® 970 Tango Black Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-65W233 Thermoplastic Elastomer
(discontinued **) A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 281-55MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | ASTM D638 |
ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | ISO 37 |
Kuraray SEPTON® S1001 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | ASTM D412 |
Momentive Performance Materials Silpruf® Construction Sealant One-part, for weatherseals, structural glazing, and general purpose sealing. Cure Method: Alkoxy (Neutral). Tack-free time 5 to 10 hr.; Peel Strength 55 lb/in.; Sag/slump 0.1 in.Data provided by the.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | ASTM D412 |
Momentive Performance Materials UltraPruf® SCS 2300 Construction Sealant One-part, for concrete, masonry, and stone. Matte finish. Cure Method: Alkoxy (Neutral); Tack-free time 5 to 10 hr. Peel Strength 55 lb/in. Sag/slump 0.1 in.Data provided by the manufacturer, GE.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | ASTM D412 |
Momentive Performance Materials IGS3723 Insulating Glass Sealant Two-component silicone which cures to form a high strength, high modulus sealant with excellent adhesion to glass. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones becam.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Through Plane Direction |
Cymat A35620SC 030SS Stabilized Aluminum Foam Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8130 Polyolefin Elastomer Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | 508 mm/min; ASTM D638 |
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer Description: ENX 7458.00 is a unique broader molecular weight distribution ethylene-butene copolymer that offers excellent flow and impact properties and is ideally suited for plastics modification... |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 141-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and has physical.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good fluid resistance and physical properties that meet ASTM F 477 for lo.. |
|||
Tensile Strength, Ultimate | 2.00 MPa | 290 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-55W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall .. |