Asahi Kasei Xyron® AT610 Modified Polyphenylene Ether

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer Asahi Kasei
Trade Name Xyron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Xyron® AT610 Modified Polyphenylene Ether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Information provided by Asahi Kasei
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
23°C
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.0 MPa
9860 psi
Flexural Modulus 2.33 GPa
338 ksi
Izod Impact, Notched 1.50 J/cm
2.81 ft-lb/in
ASTM 3.2mm
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
50% RH