Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.83 MPa @Temperature 23.0 °C |
701 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | |
Shin-Etsu Silicones KE-2090-10A/B Self-adhesive LIMS Silicone ShinEtsuKE209010 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity o.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP 1079 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-1776A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-1791R4 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP 1227A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-1357A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-2740L3-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-2740UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Monprene® MP-2815A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Telcar® TL 2530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Telcar® TL EF-6177B-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Telcar® TL-1025-65 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Telcar® TL-2448G Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D412 |
Teknor Apex Telcar® TL-2452L Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D638 |
ExxonMobil Escorene® LD 755.12 Molding, extrusion and compounding resin Escorene Ultra LD 755.12 is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | ASTM D638 |
ExxonMobil Escorene® LD 755.CM Molding, extrusion and compounding resin Escorene Ultra LD 755.CM is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl.. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Tensile Strength at Break | 4.83 MPa | 700 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDB-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |
|||
Tensile Strength at Break | >= 4.83 MPa | >= 700 psi | |
Aremco EZ-Cast™ 580N Silicon Molding Compound Silicone Rubber Aremco's EZ-Cast™ 580N is an ideal compound for producing high reliability master molds. This silicone rubber compound exhibits high tear strength, very low shrinkage and high flexibility, all requ.. |