Material Notes:
Product Description: A high crystallinity, medium impact strength copolymer resin with high melt flow rate and good processing attributes. It is designed for injection-molded automotive interior applications and large appliance parts.Availability: North America Features:Balanced Stiffness/ToughnessGood StiffnessImpact Modified NucleatedSlipUses: AppliancesAutomotive Exterior PartsAutomotive Interior PartsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.4 MPa
3250 psi
2.0 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1100 MPa
160000 psi
0.05 in/min; ASTM D790A
1260 MPa
183000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256A
Gardner Impact 26.6 J

@Thickness 3.17 mm,
Temperature -28.9 °C
19.6 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.4 °C
202 °F
ASTM D648