Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.71 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 3010 X Black Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
73°F, 0.125 in; ASTM D256
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (Cond)
Information provided by Ravago.
Izod Impact, Notched 1.71 J/cm

@Thickness 3.18 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermotuf® OF-1006 HI Polyphenylene Sulfide, Glass Fiber Reinforcement  (discontinued **)
Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ..
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
Injection Molding; ASTM D256
Network Polymers 707 Polystyrene
Description: Ignition RetardantInformation provided by Network Polymers Inc.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC
LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated.
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 206F  Nylon 12 (PA 12) Glass Fiber 35%  (discontinued **)
Glass Fiber 35%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Izod Impact, Notched 1.71 J/cm

@Thickness 3.20 mm
3.20 ft-lb/in

@Thickness 0.126 in
ASTM-D256
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256A
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)
High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren..
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Lucent Polymers GPP-330 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Lucent Polymers GPP-340 Polypropylene Homopolymer, 40% Glass Fiber Reinforced, Chemically Coupled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PA6/6 03002 CF Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact..
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
0.125 in; ASTM D256
Chase Plastics CP Pryme® A100HF ABS
Features: High FlowGeneral PurposeGood toughnessForm: PelletsInformation provided by Chase Plastics.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® A100HF ABS Molding Resin, High Flow
Information provided by Chase Plastics.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Information provided by A. Schulman.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® PC130GR Polycarbonate, 30% Glass Fiber Reinforced, Mold Release
Information provided by Chase Plastics.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Information provided by A. Schulman.
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 1499 P X 102560 A Polyphenylenesulfone (PPSU), PTFE Lubricated - Perfluoropolyether Oil
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Information provided by A. Schulman.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256A
ExxonMobil PP7855E1 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact strength copolymer resin with high melt flow rate and good processing attributes. It is designed for injection-molded automotive interior ap..
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
Aclo Accutech Polycarbonate POL050G30L Glass Reinforced
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
Aclo Accutech Polycarbonate POL051G30L Glass Reinforced
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM Test
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Dry)
Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6.
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
ASTM Test
BASF Ultramid® 8202C PA6 (Conditioned)
Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique ..
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 513 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 207 H HS MS 2 Nylon 6/6 (PA), Glass Fiber - Impact Modified - Molybdenum Disulfide - Heat Stabilized - Preliminary Data
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm
3.20 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP PA6 HI 40 GF BLK Nylon 6 (PA), Value Product - Glass Fiber - Impact Modified - Heat Stabilized
Copyright © lookpolymers.com All Rights Reserved