Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 3010 X Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.18 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermotuf® OF-1006 HI Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Rotuba H3 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM Data |
Americas Styrenics Styron® XL-8028 High Impact Polystyrene
(discontinued **) STYRON® XL-8028 high impact polystyrene is designed for VCR cassettes, toys, small appliances, telephones, housewares, tool items, computer consoles and bodies for computer cartridges. It offers hi.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1013STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.71 - 3.74 J/cm | 3.20 - 7.01 ft-lb/in | Average value: 2.30 J/cm Grade Count:5 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.20 mm |
3.20 ft-lb/in @Thickness 0.126 in |
ASTM-D256 |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256A |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers GPP-330 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | |
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PA6/6 03002 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® A100HF ABS Molding Resin, High Flow Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PC130GR Polycarbonate, 30% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.71 J/cm @Temperature 22.8 °C |
3.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Aclo Accutech Polycarbonate POL051G30L Glass Reinforced |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8202C HS PA6 (Conditioned) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8202C PA6 (Conditioned) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 513 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.71 J/cm @Temperature 22.8 °C |
3.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinelec CCB6814 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Corrugated Sheet Forms: Pellets Processing Method: Injection Method; Sheet Extr.. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.71 J/cm @Thickness 6.35 mm |
3.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |