Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1260 MPa | 183000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP7855E1 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact strength copolymer resin with high melt flow rate and good processing attributes. It is designed for injection-molded automotive interior ap.. |
|||
Flexural Modulus, 1% Secant | 1260 MPa | 183000 psi | ASTM-D790 |
Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer GD5160 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance and productivity. It was developed for the blow-molding segment. It is used in .. |
|||
Flexural Modulus, 1% Secant | 1260 MPa | 183000 psi | ASTM-D790 |
Braskem GP100BK HDPE High Density Extrusion Polyethylene GP100BK is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. It.. |