Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1260 MPa
183000 psi
0.5 in/min; ASTM D790B
ExxonMobil PP7855E1 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact strength copolymer resin with high melt flow rate and good processing attributes. It is designed for injection-molded automotive interior ap..
Flexural Modulus, 1% Secant 1260 MPa
183000 psi
ASTM-D790
Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer
GD5160 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance and productivity. It was developed for the blow-molding segment. It is used in ..
Flexural Modulus, 1% Secant 1260 MPa
183000 psi
ASTM-D790
Braskem GP100BK HDPE High Density Extrusion Polyethylene
GP100BK is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. It..