Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LL 6235 Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 6235 Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in freezer applications for food packaging.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D4883
Environmental Stress Crack Resistance <= 1.0 hour
<= 1.0 hour
Condition B, 10%; ASTM D1693
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.00 MPa
1595 psi
ASTM D638
Elongation at Break 116 %
116 %
ASTM D638
Flexural Modulus 0.250 GPa
36.2 ksi
1% secant; ASTM D790
Tensile Impact Strength 233 kJ/m²

@Temperature -40.0 °C
111 ft-lb/in²

@Temperature -40.0 °F
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
ASTM D3418
Crystallization Temperature 106 °C
223 °F
ASTM D3418
Vicat Softening Point 92.2 °C
198 °F
ASTM D1525
Brittleness Temperature >= -70.0 °C
>= -94.0 °F
ASTM D746