Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 1.0 hour | 1.0 hour | F50, Condition A, ASTM D1693 |
NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin Molded Plaque Properties. Features: High flow, Granular, Improved dispersion concentrates.Applications: housewares, additive and color, masterbatches/compounding.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 1.0 hour | 1.0 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin
(discontinued **) Molded Plaque Properties. Features: high flow.Applications: general purpose, housewares.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | <= 1.0 hour | <= 1.0 hour | Condition B, 10%; ASTM D1693 |
ExxonMobil LL 6100 Injection Molding Resin
(discontinued **) LL 6100 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications .. |
|||
Environmental Stress Crack Resistance | <= 1.0 hour | <= 1.0 hour | Condition B, 10%; ASTM D1693 |
ExxonMobil LL 6201 Injection Molding Resin
(discontinued **) LL 6201 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications .. |
|||
Environmental Stress Crack Resistance | <= 1.0 hour | <= 1.0 hour | Condition B, 10%; ASTM D1693 |
ExxonMobil LL 6235 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Environmental Stress Crack Resistance | <= 1.0 hour | <= 1.0 hour | Condition B, 10%; ASTM D1693 |
ExxonMobil LL 6235.19 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Environmental Stress Crack Resistance | <= 1.0 hour | <= 1.0 hour | F50, Condition A; ASTM D-1693 |
ExxonMobil Escorene® LD-400 LDPE Medium/High Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer resin designed for electrical applications.Applications: Base resin for medium voltage power cable insulati.. |
|||
Environmental Stress Crack Resistance | <= 1.0 hour | <= 1.0 hour | F50, Condition A; ASTM D-1693 |
ExxonMobil Escorene® LD-411 LDPE Power Cable Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer designed as an electrical grade base resin especially suitable for Henschel blending.Applications: A base r.. |
|||
Environmental Stress Crack Resistance | 1.0 hour @Pressure 2.50 MPa |
1.0 hour @Pressure 363 psi |
ISO CD 16770 |
Iran Petrochemical (PCC) I2 HB 7250 High Density Polyethylene I2 (HB 7250) is a high density polyethylene with Propylene as comonomer. It is easy flowing, low warpage, less hard and stiff than I1.Applications: household articles, closures/seals, packaging.Info.. |
|||
Environmental Stress Crack Resistance | >= 1.0 hour @Temperature 50.0 °C |
>= 1.0 hour @Temperature 122 °F |
Igepal 10%;F20; IEC 60811-4-1/B |
Borealis FR4810 Low Smoke Zero Halogen Flame Retardant Jacketing Compound FR4810 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, black jacketing compound combining with flexibility and exceptional fluid resistance. The composition is based on the elemen.. |
|||
Environmental Stress Crack Resistance | 1.0 hour @Pressure 0.920 MPa, Temperature 80.0 °C |
1.0 hour @Pressure 133 psi, Temperature 176 °F |
ISO 13479 |
Borealis BorSafe™ HE3490-IM HDPE Compound for Injection Molded Pressure Fittings BorSafe™ HE3490-IM is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by .. |