Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 124 °C | 255 °F | Internal method |
Polimeri Europa Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexi.. |
|||
Melting Point | 124 °C | 255 °F | Internal method |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
Melting Point | 124 °C | 255 °F | Internal method |
Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Melting Point | 124 °C | 255 °F | 10°C/min; ISO 11357-1/-3 |
DSM Yparex® 8104 R Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melting Point | 124 °C | 255 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1237x98 Cast Film Resin
(discontinued **) LL 1237x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Melting Point | 124 °C | 255 °F | ASTM D3418 |
ExxonMobil LL 6235 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Melting Point | 124 °C | 255 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3002.32 Cast Film Resin
(discontinued **) LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, .. |
|||
Melting Point | 124 °C | 255 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3105.50 Premium High Strength Film Resin
(discontinued **) LL 3150.32 is a hexene copolymer LLDPE film resin for blown film. Films produced from this resin have excellent tensile and toughness properties, as well as improved stiffness. Combined with good dr.. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin, 0.6 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Melting Point | 124 °C | 255 °F | |
M. Holland Company MAGMA® LL1091 LLDPE
(discontinued **) Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | 124 °C | 255 °F | 10°C/min; ISO 11357-1/-3 |
Yparex 8102 Polyolefin Adhesive Resin The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melting Point | 124 °C | 255 °F | NOVA |
NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin Features: Excellent processabilityGood stiffness and strengthHigh stretchability Applications: Overwrap filmNettingBlend resinInformation provided by Nova Chemicals |
|||
Melting Point | 124 °C | 255 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5069 400 Micron LLDPE Powder Description: ICOFLO 510-5069 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 124 °C | 255 °F | Eutectic |
Indium Corp. Indalloy® 255 Bi-Pb Fusible Alloy General purpose fusible alloy. Poor solderability.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 124 °C | 255 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M735 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cycle.. |
|||
Melting Point | >= 124 °C | >= 255 °F | ISO 11357/03 |
Borealis Borstar® FB2230 LLDPE for Film Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Melting Point | 124 °C | 255 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3001.32 Cast Film Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Melting Point | 124 °C | 255 °F | Equate Test Method |
Equate EFDA-7047 LLDPE Film Extrusion Resin EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does n.. |
|||
Melting Point | 124 °C | 255 °F | Equate Test Method |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |
|||
Melting Point | 124 °C | 255 °F | Equate Test Method |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow DOWLEX™ 2083G Linear Low Density Polyethylene Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 124 °C | 255 °F | |
Arkema Group Orevac® 18303S Maleic Anhydride modified LLDPE LLDPE base Composition: PE / Adh./ EVOH Applications:Flooring Heating TubeInformation provided by Arkema Group |
|||
Melting Point | 124 °C | 255 °F | ASTM-D3418 |
Braskem RD34U3 LLDPE Rotomolding Polyethylene The resin RD34U3 is a linear low-density polyethylene, 1-butene based, with excellent processability and a good balance of stiffness and impact strength. It contains long term UV6 stabilization and .. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Melting Point | 124 °C | 255 °F | ASTM D3417 |
Total Finacene® BM359SG HDPE, blow molding
(Unverified Data**) FINACENE® BM359 SG has been especially designed for the manufacture of blow moulded bottles (up to 5 liters) with a superior surface gloss and contact transparency. It is recommended either in mono.. |
|||
Melting Point | 124 °C | 255 °F | ASTM D3417 |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |
|||
Melting Point | 124 °C | 255 °F | 10°C/min; ISO 11357-1/-3 |
DSM Yparex® 8403 RS Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |