Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.00 MPa | 1595 psi | ASTM D638 |
ExxonMobil LL 6100 Injection Molding Resin
(discontinued **) LL 6100 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications .. |
|||
Tensile Strength, Yield | 11.00 MPa | 1595 psi | ASTM D638 |
ExxonMobil LL 6235 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Tensile Strength, Yield | 11.00 MPa | 1595 psi | ASTM D638 |
ExxonMobil LL 6235.19 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |