Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ BMU 234 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMU 234 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, South America and North America Features: Good Creep ResistanceGood Dimensional StabilityGood Impact ResistancePaintableUltra High Stiffness Uses: Automotive ApplicationsAutomotive Exterior Parts Automotive Exterior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.4 MPa
2090 psi
ISO 527-2
Tensile Strength, Yield 18.5 MPa
2680 psi
ISO 527-2
Tensile Modulus 1.84 GPa
267 ksi
Secant; ISO 527-2
Flexural Modulus 1.85 GPa
268 ksi
ISO 178
Charpy Impact, Notched 0.441 J/cm²

@Temperature -30.0 °C
2.10 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
0.546 J/cm²

@Temperature -20.0 °C
2.60 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
0.735 J/cm²

@Temperature 0.000 °C
3.50 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 53.9 °C
129 °F
ISO 75-2/A
Copyright © lookpolymers.com All Rights Reserved