Mechanical Properties Metric English Comments
Tensile Modulus 1.84 GPa
267 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics GELOY CR3020 ASA
Low-gloss ASA for profile and capstock applications
Tensile Modulus 1.84 GPa
267 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Konduit MT00EL PP
LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th..
Tensile Modulus 1.84 GPa
267 ksi
ISO 527
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific)
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 1.84 GPa
267 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Tensile Modulus 1.84 GPa
267 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS
LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release.
Tensile Modulus 1.84 GPa
267 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea..
Tensile Modulus 1.84 GPa

@Temperature 110 °C
267 ksi

@Temperature 230 °F
50%RH; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..
Tensile Modulus 1.84 GPa
266 ksi
Storage
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy
Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of..
Tensile Modulus 1.84 GPa
267 ksi
same value from ASTM and ISO test.
BASF Capron® BU50I Ultratough Nylon 6 (Dry)  (discontinued **)
Capron Ultratough Nylon BU50I is an unfilled nylon 6 product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU5..
Tensile Modulus 1.84 GPa
267 ksi
1mm/min
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Tensile Modulus 1.84 GPa

@Temperature 30.0 °C
267 ksi

@Temperature 86.0 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont ..