Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.60 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.546 J/cm²

@Temperature -30.0 °C
2.60 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMT222 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by good stiffness/toughness balance and designed for automotive interior applications in which good surface finish and g..
Charpy Impact, Notched 0.546 J/cm²

@Temperature -30.0 °C
2.60 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 133 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for paintable automotive exterior applications.Availability: Europe ..
Charpy Impact, Notched 0.546 J/cm²

@Temperature -20.0 °C
2.60 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea..
Charpy Impact, Notched 0.546 J/cm²

@Temperature 0.000 °C
2.60 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol..
Charpy Impact, Notched 0.546 J/cm²

@Temperature 0.000 °C
2.60 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac..
Charpy Impact, Notched 0.546 J/cm²

@Temperature 0.000 °C
2.60 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
ExxonMobil PP7064L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain..
Copyright © lookpolymers.com All Rights Reserved