Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 97.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
Unannealed; ASTM D648
Multibase Nylex™ 2185 HF Polyamide + PP
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylac® GP55 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
ASTM D648
Plaskolite Optix® DA Digital Acrylic Sheet
Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup..
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylac® EX28 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
Unannealed; ASTM D648
M. Holland Company CP402 Polypropylene Impact Copolymer
Impact copolymerGood impact resistanceLow temperature impact resistanceNucleatedGood stiffnessApplications: CratesLawn and garden equipmentTool/tote box
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
ASTM D648
Ineos H19G-01 Polypropylene Homopolymer
Grade H19G-01 is a polypropylene homopolymers designed for extrusion processing and meet the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.Applications:Contin..
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
Unannealed; ASTM D648
Global PP-2300-SC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-thin walled parts, electrical appliancesInformation provided by Global Polymers Corporation.
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
Unannealed; ISO 75B-1, -2
LyondellBasell Hifaxâ„¢ HSBMG265 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ HSBMG265 medium high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of rigidity, ..
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
ISO 75-2/B
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea..
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
ASTM D648
Aclo Accutech Polypropylene Copolymer CP0437M30L Mica Reinforced
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
ASTM D648
Americas Styrenics EA3130 High Heat Crystal Polystyrene
Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC.
Deflection Temperature at 0.46 MPa (66 psi) 97.2 - 149 °C
207 - 300 °F
Average value: 122 °C Grade Count:21
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..
Copyright © lookpolymers.com All Rights Reserved