ExxonMobil Escorene® LD-702 High EVA Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-702 High EVA Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and toughness.Applications: Pallet stretch wrap; Heat seal layer in coextruded or laminated structures; Liquid packaging; Profile extrusions; Compounding; Frozen food bags.
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 0.30 g/10 min
0.30 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Hardness, Shore D 33
33
ASTM D2240
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0830 GPa
12.0 ksi
1% Secant, ASTM D790
Tensile Impact Strength 773 kJ/m²
368 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 92.0 °C
198 °F
Exxon Method
Vicat Softening Point 77.0 °C
171 °F
1000g; ASTM D-1525