Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0828 GPa | 12.0 ksi | 1% Sec; ASTM D-790-92 |
Multibase Multi-Flex® TPE A 8502 EXCEL GREY Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® CHP-010 Thermoplastic Polyolefin
(discontinued **) Applications: Soft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Flexural Modulus | 0.0827 GPa | 12.0 ksi | ASTM D790 |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Flexural Modulus | 0.0827 GPa | 12.0 ksi | |
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-705 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Base resin for fully formulated low voltage cable i.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
3M Dyneon™ THV™ 200P Fluorothermoplastic, Powder Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
3M Dyneon™ THV™ 200G Fluorothermoplastic, Pellet Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Flexural Modulus | 0.0827 GPa | 12.0 ksi | ASTM D790 |
Multibase Multi-Flex® A 8030 C2 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flexural Modulus | 0.0827 GPa | 12.0 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® A 8502 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Moldability, GoodPaintable Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsInforma.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.0827 GPa | 12.0 ksi | ASTM D790 |
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Flexural Modulus | 0.0827 GPa | 12.0 ksi | ASTM D790 |
Ecomass® 4703ZD90 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-702 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |