Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.943 g/cc | 0.0341 lb/in³ | |
Plastcom SLOVALEN EQ 18 N PP, basic type FeaturesModified PE with special heat and processional stabilization. Application in extrusion of profiles and pipes, blowing of bottles and jerrycans. Delivered in black colour.Packaging, transport.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Reliance Industries Relene W43006 Polyethylene Relene W43006 is a polyethylene grade recommended for insulation in jelly filled telecommunication cables. This grade contains a special stabilization system for improved thermal resistance. It is.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2209 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Reliance Industries Relene E41003 Polyethylene Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial eff.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Reliance Industries Relene L41003 Polyethylene The UV stabilized version of Relene E41003Information provided by Reliance Industries |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 8406 BK, 8406 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin
(discontinued **) Resin Type: Melt blend, FDA approvedCharacteristics: Good processabilityGood drawdown capabilityImproved MVTR propertiesGrease resistanceApplications: MVTR applicationsRelease linersCup stockInforma.. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 293-285 High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 293-285D High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 297-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 297-285D High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX2250 Extrudable Tie-Layer Resin, Anhydride Modified HDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 155-1339 LMDPE Rotational Molding Resin Description: ICORENE 155-1339 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) BL5 HM 7746 High Density Polyethylene BL5 (HM 7746) is a high density polyethylene with Butene-1 as comonomer. It is a high molar mass, very good impact strength and optimum stress cracking resistance.Applications: large containers abov.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Micropol Microlink XL28 Crosslinkable Polyethylene Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact), ESCR, chemical, a.. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 293-285SK High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR590005 High Density Polyethylene ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains .. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | base resin; ISO 1872-2/ISO 1183 |
Borealis Borcell™ HE1346 High Density Polyethylene Borcell™ HE1346 is a fully formulated compound for chemical foamed telesingles. Borcell™ HE1346 is a high-density polyethylene compound containing chemical blowing agent.
Applications Borcell™ HE.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ISO 1183 |
Borealis BorSafe™ ME3445 Medium Density Polyethylene BorSafe™ ME3445 is a bimodal polyethylene compound produced by the advanced Borstar® technology. It's fully stabilized against thermal degradation and the die build-up during extrusion is minimiz.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D792 |
DuPont Bynel® 3101 Acid-/Acrylate-Modified EVA Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM-D5 |
Westlake Epolene® E-16 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D4883 |
Westlake Tymax™ GT7058 Anhydride Modified Acrylate Copolymer Westlake GT7058 is an anhydride modified acrylate copolymer designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a coextruded tie.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D-1505 |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ExxonMobil Method |
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ExxonMobil method |
ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin Product Description: Polybilt 101 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 10.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM-D792 |
Braskem LL3800N HDPE Cast Film Extrusion Polyethylene Copolymer The resin LL3800N is a high-density polyethylene, copolymer octene-1, produced by the solution process for the extrusion of plain films with excellent mechanical properties. It has an antirust addit.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-702 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |
|||
Density | 0.943 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Reliance Industries Relene B31101 Polyethylene Steel pipe coating base High Density Polyethylene resin. Characteristics:broad molecular weight distribution, good melting strength, excellent toughness/ESCR, and good cut through/abrasion resistanc.. |