Polymer Property : Melting Point = 92.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 92.0 °C
198 °F
Internal Method
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion
Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: ..
Melting Point 92.0 °C
198 °F
Freezing Point, DSC; ASTM D3418
DuPont Bynel® 30E699 Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 92.0 °C
198 °F
Exxon Method
ExxonMobil Escorene® LD-705 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t..
Melting Point 92.0 - 121 °C
198 - 250 °F
Indium Corp. Indalloy 63 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 92.0 °C
198 °F
Freezing Point via DSC/ASTM D3418
DuPont 20 Series DPE 20 Specialty Polyethylene Resin
DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex..
Melting Point 92.0 °C
198 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process ..
Melting Point 92.0 °C
198 °F
By DSC; ASTM D3418 - ISO 3146
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer
Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go..
Melting Point 92.0 °C
198 °F
Upon Melting via DSC/ASTM D3418
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 92.0 °C
198 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res..
Melting Point 92.0 °C
198 °F
TRN-14
Tipco Tipcolite® TPF 1312 - Unreinforced Thermoset Phenolic Resin, 21 mm Norton Flow with 13% Hexamine
Unreinforced Phenolic Resin having 21mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Melting Point 92.0 °C
198 °F
ISO 11357
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: ..
Melting Point 92.0 °C
198 °F
DSC; ASTM D3418
DuPont Appeel® LSR20D745 Lidding Sealant Resin
Appeel® LSR20D745 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu..
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
DuPont™ Appeel® 20D855 Ethylene Acrylate
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
DuPont™ Bynel® 22E757 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
DuPont™ Entira® AS500 Ionomer Resin
Entira™ AS MK400 is used to lower the static decay time and surface resistivity of polyolefins and other polymers. Entira™ AS MK400 can be precompounded or dry blended into polymers for extrusion,..
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
DuPont™ Entira® ASSD100 Ionomer Resin
DuPont™ Entira™ AS SD100 is an extremely hygroscopic ionomer resin that is supplied as free flowing pellets. Entira™ AS SD100 is used to lower the static decay time and surface resistivity of LD..
Melting Point 92.0 °C
198 °F
DTA
DuPont™ Surlyn® 9650 Ionomer Resin, Zinc
Surlyn® 9650 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Melting Point 92.0 °C
198 °F
DTA
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc
Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Melting Point 92.0 °C
198 °F
DTA
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc
Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Melting Point 92.0 °C
198 °F
10°C/min
Arkema Group Evatane® 1040 VN 4 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and high mechanical properties. Examples: thin stretch film for food packaging, coex..
Melting Point 92.0 °C
198 °F
DSC
Arkema Group LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 14 MGC 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the Methyl Acrylate content, LOTRYL® 14 MGC 02 is a polymer o..
Melting Point 92.0 °C
198 °F
ASTM D3417, ISO 3146
DuPont™ Surlyn® 1707 Sodium Ionomer
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Melting Point 92.0 °C
198 °F
Exxon Method
ExxonMobil Escorene® LD-702 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t..
Melting Point 92.0 °C
198 °F
Eutectic
Indium Corp. Indalloy 197 Bismuth Solder Alloy
Information Provided by Indium Corporation