Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Water Absorption 0.010 %

@Temperature 23.0 °C,
Time 86400 sec
0.010 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 4.00 mm
0.0020 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 56.0 MPa
8120 psi
5 mm/min; ISO 527
Elongation at Break 2.5 %
2.5 %
5 mm/min; ISO 527
3.7 %
3.7 %
Flexural, 5 mm/min; ISO 178
Tensile Modulus 5.40 GPa
783 ksi
1 mm/min; ISO 527
Flexural Strength 45.0 MPa
6530 psi
2 mm/min; ISO 178
Flexural Yield Strength 86.0 MPa
12500 psi
2 mm/min; ISO 178
Flexural Modulus 5.40 GPa
783 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 44.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
24.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 127 µm/m-°C

@Temperature 23.0 - 60.0 °C
70.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 195 - 205 °C
383 - 401 °F
Zone 2 215 - 225 °C
419 - 437 °F
Zone 3 225 - 250 °C
437 - 482 °F
Melt Temperature 225 - 250 °C
437 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved