Material Notes:
Engineered for high temperature and high impact resistance.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. Very good impact resistance. Good thermal shock resistance. Military Spec MIL-A-46050C Type 2. Military Spec MIL-A-46050C Class 2. A primer is required for hard-to-bond materials such as polyethylene, polypropylene, acetal, PET, nylon, soft PVC, silicone rubber, and glass.General information about the Aron Alpha® product line: Cyanoacrylates are single component instant adhesives that bond a wide variety of surfaces with a strong, durable bond. They offer ease of application, a wide range of performance parameters, and reliable solvent-free bonding.Toagosei Co., Ltd. produces cyanoacrylates in Japan, marketed as Aron Alpha® in Japan, Cyanolit® in Europe, and Krazy Glue® in the US. Elmer's Products markets Krazy Glue® to the retail trade and Aron Alpha® to the industrial trade in North America. Information provided by Elmer's Products, Inc.
Physical Properties Metric English Comments
Viscosity 2.0 cP
2.0 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
34.5 MPa
5000 psi
vs. rigid PVC; 5 s set time
34.5 MPa
5000 psi
vs. polycarbonate; 20 s set time
40.0 MPa
5800 psi
vs. steel; 15 s set time
40.0 MPa
5800 psi
vs. aluminum; 15 s set time
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Estimated; Manufacturer specifies clear but does not quantify.
Processing Properties Metric English Comments
Processing Temperature 20.0 °C
68.0 °F
typically used at ambient temperature
Descriptive Properties Value Comments
Color Clear